Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Density / Specific Gravity | | ASTMD792 | 1.51 | g/cm³ |
Melt Mass-Flow Rate | 337°C/6.6kg | ASTMD1238 | 5.0 | g/10min |
Modeling Shrinkage | MD:3.20mm | 内部方法 | 0.20to0.40 | % |
Modeling Shrinkage | TD:3.20mm | 内部方法 | 0.20to0.40 | % |
Moisture Absorption | 24hr | ASTMD570 | 0.16 | % |
Moisture Absorption | Equilibrium,23°C | ASTMD570 | 0.90 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Modulus | | ASTMD638 | 9310 | Mpa |
Tensile Strength | Yield | ASTMD638 | 169 | Mpa |
Tensile Strength | Break | ASTMD638 | 159 | Mpa |
Tensile Elongation | Break | ASTMD638 | 3.0 | % |
Flexural Modulus | 100mmSpan | ASTMD790 | 8960 | Mpa |
Flexural Strength | Break,100mmSpan | ASTMD790 | 228 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Heat Deflection Temperature | 0.45MPa,Unannealed,6.40mm | ASTMD648 | 212 | °C |
Heat Deflection Temperature | 1.8MPa,Unannealed,6.40mm | ASTMD648 | 210 | °C |
Vicat Softening Temperature | | ASTMD15255 | 228 | °C |
Coefficient of Linear Thermal Expansion | MD:-20to150°C | ASTME831 | 2E-05 | cm/cm/°C |
RTIElec | | UL746 | 180 | °C |
RTIImp | | UL746 | 170 | °C |
RTIStr | | UL746 | 180 | °C |
Electrical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Volume Resistivity | | ASTMD257 | 3E+16 | ohms·cm |
Dielectric Strength | 1.60mm,inAir | ASTMD149 | 25 | KV/mm |
Dielectric Strength | 1.60mm,in Oil | ASTMD149 | 30 | KV/mm |
Dielectric Constant | 1kHz | ASTMD150 | 3.70 | |
Dissipation Factor | 1kHz | ASTMD150 | 1.5E-03 | |
Dissipation Factor | 2.45GHz | ASTMD150 | 5.3E-03 | |
Arc Resistance | | ASTMD495 | PLC6 | |
Comparative Tracking Index | CTI | UL746 | PLC4 | |
High Amp Arc Ignition | HAI | UL746 | PLC4 | |
High Voltage Arc Tracking Rate | HVTR | UL746 | PLC3 | |
Hot-wire Ignition | HWI | UL746 | PLC1 | |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|
Notched Izod Impact Strength | 23°C | ASTMD256 | 85 | J/m |
Notched Izod Impact Strength | 23°C | ASTMD4812 | 430 | J/m |
Reverse Notch Izod Impact | 3.20mm | ASTMD256 | 490 | J/m |
Hardness | Test Condition | Test Method | Test Result | Unit |
---|
Rockwell Hardness | M-Scale | ASTMD785 | 114 | |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|
Flame Rating | 0.25mm | UL94 | V-0 | |
Flame Rating | 1.2mm | UL94 | 5VA | |
Oxygen Index | | ASTMD2863 | 50 | % |
NBSSmokeDensity-Flaming,Ds,4min | | ASTME662 | 1.60 | |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.