Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Density / Specific Gravity | | ASTMD792 | 1.30到1.32 | g/cm³ |
Melt Mass-Flow Rate | 250°C/2.16kg | ASTMD1238 | 23到30 | g/10min |
Color b | | Q/KHS001 | 1.00到3.00 | |
ColorL | | Q/KHS001 | >95.0 | |
ParticleMass | | Q/KHS001 | 1.90到2.10 | g/100pcs |
Solid Content | | Q/KHS001 | 0.99到1.0 | dl/g |
Moisture Content | | Q/KHS001 | <0.20 | wt% |
Ash Content | | Q/KHS001 | <300 | mg/kg |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Strength | | ASTMD638 | 50.0到60.0 | Mpa |
Tensile Elongation | Break | ASTMD638 | >150 | % |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Melting Temperature | | Q/KHS001 | >222 | °C |
Electrical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Dielectric Strength | 2.00mm | ASTMD149 | >20 | KV/mm |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|
Notched Izod Impact Strength | | ASTMD256 | >39 | J/m |
Additional | Test Condition | Test Method | Test Result | Unit |
---|
CarboxylEndGroups | | Q/KHS001 | <24.0 | mol/t |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.