PMMA LGMMA® HI-835MS LX MMA KOREA
296
- Unit Price:US$ 3,169 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:10MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:wear resistant|High temperature resistance
- Application Areas:Spray free applications|Automotive components
- Color:--
- Grade:Injection grade
Technical Data Sheet
| optical performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Refractive index | ASTM D542 | 1.490 | |
| transmissivity | 3200μm | ASTM D1003 | 90.0 % |
| turbidity | 3200μm | ASTM D1003 | <1.0 % |
| impact performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Charpy Notched Impact Strength | ISO 179/1eA | 4.0 kJ/m² | |
| Impact strength of simply supported beam without notch | ISO 179/1eU | 40 kJ/m² | |
| Impact strength of cantilever beam gap | Area | ASTM D256 | 3.70 kJ/m² |
| flammability | Test Condition | Test Method | Test Result |
|---|---|---|---|
| UL flame retardant rating | UL 94 | HB |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| bending strength | Yield | ASTM D790 | 86.3 Mpa |
| tensile strength | Yield | ASTM D638 | 48.1 Mpa |
| elongation | Yield | ASTM D638 | 85 % |
| Bending modulus | ASTM D790 | 2140 Mpa |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa,Unannealed | ASTM D648 | 84.0 °C |
| Vicat softening temperature | ASTM D15252 | 98.0 °C | |
| Linear coefficient of thermal expansion | MD | ASTM D696 | 7E-05 cm/cm/°C |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| density | ASTM D792 | 1.17 g/cm³ | |
| melt mass-flow rate | 230°C/3.8kg | ASTM D1238 | 2.7 g/10min |
| Shrinkage rate | MD | ASTM D955 | 0.40-0.80 % |
| Water absorption rate | 24hr | ASTM D570 | 0.40 % |
| Electrical performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Dielectric constant | 60Hz | ASTM D150 | 3.10 |
| Dissipation factor | 60Hz | ASTM D150 | 0.040 |
| Volume resistivity | ASTM D257 | >1.0E+15 ohms·cm | |
| Dielectric strength | ASTM D149 | 15 KV/mm |
| hardness | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Rockwell hardness | M-Scale | ASTM D785 | 61 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.