Material Description
- Material Properties:Glass fiber reinforced|High impact resistance
- Application Areas:Automotive Applications|Profile
- Color:--
- Grade:Injection grade
Technical Data Sheet
| optical performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| gloss | 60° | ISO 2813 | 130 |
| Gelboflex test | Internal Method | 200 holes/m² | |
| ISO Type | ISO 1874 | PA 66/610, FT, 18-030 |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Melting temperature | ISO 11357-3 | 200 °C |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Melt Volume Flow Rate (MVR) | 275°C/5.0 kg | ISO 1133 | 40.0 cm3/10min |
| Water absorption rate | Saturation, 23°C | ISO 62 | 6.0 % |
| Equilibrium, 23°C, 50% RH | ISO 62 | 2.5 % |
| film | Test Condition | Test Method | Test Result |
|---|---|---|---|
| tensile strength | MD : Yield | ISO 527-3 | 30.0 Mpa |
| TD : Yield | ISO 527-3 | 28.0 Mpa | |
| MD : Break | ISO 527-3 | 70.0 Mpa | |
| TD : Break | ISO 527-3 | 60.0 Mpa | |
| elongation | MD : Yield | ISO 527-3 | 10 % |
| TD : Yield | ISO 527-3 | 10 % | |
| MD : Break | ISO 527-3 | 900 % | |
| TD : Break | ISO 527-3 | 900 % | |
| Elmendorf tear strength | MD | ISO 6383-2 | 20 N |
| TD | ISO 6383-2 | 20 N | |
| Tear resistance of pants type | MD | ISO 6383-1 | 50.0 N/mm |
| TD | ISO 6383-1 | 75.0 N/mm | |
| Water vapor permeability | 23°C, 85% RH | DIS 15106-1/-2 | 20 g/m²/24 hr |
| Oxygen permeability | 23°C2 | ASTM D256A | 25 cm³/m²/bar/24 hr |
| 23°C3 | ASTM D256A | 70 cm³/m²/bar/24 hr | |
| Carbon dioxide transmittance | 23°C2 | ASTM D256A | 80.0 cm³/m²/bar/24 hr |
| 23°C3 | ASTM D256A | 250 cm³/m²/bar/24 hr |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.