PC 4800-10 STYRON TAIWAN
138
- Unit Price:US$ 2,233 /MT
- Packaging Specification:
- Supply Quantity:31MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
- Material Comparison:
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:High impact resistance
- Application Areas:Electrical field|Electronic field
- Color:--
- Grade:Flame retardant grade
Technical Data Sheet
| Other performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Glow wire combustion index (GWFI) | 2.0mm | IEC 695-2-1 | 960 °C |
| Limiting Oxygen Index (LOI) | ASTM D-2863 | 36 % |
| Basic Performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| melt mass-flow rate | 300℃/1.2kg | ASTM D-1238 | 10 g/10min |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| tensile strength | Break | ASTM D-638 | 59 Mpa |
| Impact strength of cantilever beam gap | 总能量@23℃ | ASTM D-1822 | 631 KJ/m |
| Rockwell hardness | ASTM D-785 | 59 M Scale | |
| tensile strength | Yield | ASTM D-638 | 61 Mpa |
| Bending modulus | ASTM D-790 | 2330 Mpa | |
| bending strength | ASTM D-790 | 98 Mpa | |
| elongation | Break | ASTM D-638 | 115 % |
| Impact strength of cantilever beam gap | 23℃ | ASTM D-256 | 未破裂 |
| Tensile modulus | ASTM D-638 | 2380 Mpa | |
| Impact strength of cantilever beam gap | 23℃ | ASTM D-256 | 694 J/m |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Vicat softening temperature | 50℃/hr,50n重 | ASTM D-1525 | 151 °C |
| Hot deformation temperature | Annealed@0.45MPa | ASTM D-648 | 137 °C |
| Shrinkage rate | ASTM D-696 | 65×10 mm/mm/℃ | |
| Hot deformation temperature | Unannealed@1.82MPa | ASTM D-648 | 127 °C |
| Ball indentation temperature | IEC 598-1 | >125 °C |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Shrinkage rate | ASTM D-955 | 0.005-0.007 mm/mm |
| Electrical performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Compared to the Leakage Traceability Index (CTI) | 2.0mm | IEC 112 | 225 V |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.