PA66 Ultramid® A3WG10 BASF GERMANY
363
- Unit Price:US$ 4,786 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:60MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:Oil resistant|Dimensional stability|High rigidity|heat-resisting|Filler: Glass fiber reinforced material|50% filler by weight
- Application Areas:Industrial applications
- Color:--
- Grade:Enhanced level
Material Certification

Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Charpy Notched Impact Strength | -30°C | ISO 179 | 13 kJ/m² |
| 23°C | ISO 179 | 15 kJ/m² | |
| Impact strength of simply supported beam without notch | -30°C | ISO 179 | 85 kJ/m² |
| 23°C | ISO 179 | 95 kJ/m² | |
| Impact strength of cantilever beam gap | -40°C | ISO 180 | 14 kJ/m² |
| 23°C | ISO 180 | 17 kJ/m² |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Tensile modulus | 23°C | ISO 527-2 | 17000 Mpa |
| tensile strength | Break,23°C | ISO 527-2 | 240 Mpa |
| Tensile strain | Break,23°C | ISO 527-2 | 2.5 % |
| Bending modulus | 23°C | ISO 178 | 15300 Mpa |
| bending strength | 23°C | ISO 178 | 360 Mpa |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 256 °C |
| Melting temperature | ISO 3146 | 260 °C | |
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 262 °C |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| density | ISO 1183 | 1.57 g/cm³ | |
| Shrinkage rate | TD | ISO 294-4 | 1.0 % |
| MD | ISO 294-4 | 0.40 % | |
| Water absorption rate | Saturation,23°C | ISO 62 | 4.0 % |
| Equilibrium,23°C,50%RH | ISO 62 | 1.2 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.