plas

PC/PET XYLEX™  X7300CL SABIC INNOVATIVE US

385
  • Unit Price:US$ 3,493 /MT
  • Packaging Specification:
    25 KG/PKG
  • Packaging Material:
    Paper bag
  • Supply Quantity:
    72MT
  • Delivery Terms:
    FOB
  • Port of Loading :
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 ********View
serv********View
+86 ********View

For more details, please contact the supplier!

Material Description

  • Material Properties:UV resistanceHigh mobility
  • Application Areas:Automotive sector
  • Color:--
  • Grade:Injection grade

Technical Data Sheet

optical performanceTest ConditionTest MethodTest Result
transmissivity2540μmASTM D100388.0 %
turbidity2540μmASTM D10032.0 %
impact performanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gap23°CISO 180/1A9.0 kJ/m²
Dart impact23°C,TotalEnergyASTM D376395.0 J
mechanical propertiesTest ConditionTest MethodTest Result
Tensile modulusASTM D6381840 Mpa
Tensile modulusISO 527-2/11900 Mpa
tensile strengthYieldASTM D63849.0 Mpa
tensile strengthYieldISO 527-2/5055.0 Mpa
tensile strengthBreakASTM D63852.0 Mpa
tensile strengthBreakISO 527-2/5055.0 Mpa
elongationYieldASTM D6385.0 %
Tensile strainYieldISO 527-2/505.0 %
elongationBreakASTM D638150 %
Tensile strainBreakISO 527-2/50>150 %
Bending modulus50.0mmSpanASTM D7901940 Mpa
Bending modulusISO 1782000 Mpa
bending strengthISO 17871.0 Mpa
bending strengthYield,50.0mmSpanASTM D79083.0 Mpa
thermal performanceTest ConditionTest MethodTest Result
Linear coefficient of thermal expansionTD:-40to40°CASTME8311.1E-04 cm/cm/°C
Linear coefficient of thermal expansionTD:23to60°CISO 11359-28.5E-05 cm/cm/°C
Hot deformation temperature0.45MPa,Unannealed,3.20mmASTM D648102 °C
Hot deformation temperature1.8MPa,Unannealed,3.20mmASTM D64888.0 °C
Hot deformation temperature1.8MPa,Unannealed,100mmSpanISO 75-2/Ae90.0 °C
Vicat softening temperatureASTM D15259108 °C
Vicat softening temperatureISO 306/B120106 °C
Linear coefficient of thermal expansionMD:-40to40°CASTME8311.2E-04 cm/cm/°C
Linear coefficient of thermal expansionMD:23to60°CISO 11359-28.5E-05 cm/cm/°C
Physical propertiesTest ConditionTest MethodTest Result
melt mass-flow rate265°C/2.16kgASTM D123821 g/10min
Melt Volume Flow Rate (MVR)265°C/2.16kgISO 113321.0 cm3/10min
Shrinkage rateMD:3.20mmInternal Method0.40-0.80 %
Shrinkage rateTD:3.20mmInternal Method0.50-0.70 %
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.