plas

PC PANLITE® MN-3600H TEIJIN JAPAN

442
  • Unit Price:US$ 2,816 /MT
  • Packaging Specification:
    25 KG/PKG
  • Packaging Material:
    Paper bag
  • Supply Quantity:
    41MT
  • Delivery Terms:
    FOB
  • Port of Loading :
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 ********View
serv********View
+86 ********View

For more details, please contact the supplier!

Material Description

  • Material Properties:heat-resistingFlame retardantGood impact resistanceGood liquidityHalogen-free
  • Application Areas:Electrical fieldElectronic fieldAutomotive sector
  • Color:--
  • Grade:Injection grade

Material Certification

UL

Technical Data Sheet

otherTest ConditionTest MethodTest Result
remarks以上加工数据.为参考值.以生产厂商设备的实际状况而进行调整
characteristic抗撞击性良好、耐热性高、良好的流动性、无卤、阻燃性能
Color不透明
purpose电气/电子应用领域、汽车领域的应用
impact performanceTest ConditionTest MethodTest Result
Impact strength of simply supported beam without notchISO 179NoBreak
flammabilityTest ConditionTest MethodTest Result
Burning wire flammability index3.0mmIEC 60695-2-12930 °C
Hot filament ignition temperature1.0mmIEC 60695-2-13875 °C
Hot filament ignition temperature1.5mmIEC 60695-2-13825 °C
Hot filament ignition temperature2.0mmIEC 60695-2-13825 °C
Hot filament ignition temperature3.0mmIEC 60695-2-13825 °C
UL flame retardant rating0.45mmUL 94HB
UL flame retardant rating1.0mmUL 94V-1
UL flame retardant rating1.5mmUL 94V-0
UL flame retardant rating2.0mmUL 945VB
UL flame retardant rating3.0mmUL 945VA
Burning wire flammability index1.0mmIEC 60695-2-12960 °C
Burning wire flammability index1.5mmIEC 60695-2-12930 °C
Burning wire flammability index2.0mmIEC 60695-2-12960 °C
mechanical propertiesTest ConditionTest MethodTest Result
Tensile modulusASTM D638/ISO 5272350 kg/cm²(MPa)[Lb/in²]
tensile strengthASTM D638/ISO 52760.0 kg/cm²(MPa)[Lb/in²]
elongationASTM D638/ISO 5277.0 %
Bending modulusASTM D790/ISO 1782300 kg/cm²(MPa)[Lb/in²]
bending strengthASTM D790/ISO 17895.0 kg/cm²(MPa)[Lb/in²]
Elongation at BreakASTM D638/ISO 527100 %
Bending modulusISO 1782300 Mpa
bending strengthISO 17895.0 Mpa
Tensile modulusISO 527-2/12350 Mpa
tensile strengthYieldISO 527-2/5060.0 Mpa
tensile strengthBreakISO 527-2/5050.0 Mpa
Tensile strainYieldISO 527-2/507.0 %
Tensile strainBreakISO 527-2/50100 %
thermal performanceTest ConditionTest MethodTest Result
Hot deformation temperatureHDTASTM D648/ISO 75125 ℃(℉)
Linear coefficient of thermal expansionASTM D696/ISO 113590.000070 mm/mm.℃
RTI Str1.5mmUL 74695.0 °C
Hot deformation temperature0.45MPa,UnannealedISO 75-2/B125 °C
Hot deformation temperature1.8MPa,UnannealedISO 75-2/A112 °C
Linear coefficient of thermal expansionMDISO 11359-27E-05 cm/cm/°C
Linear coefficient of thermal expansionTDISO 11359-27E-05 cm/cm/°C
RTI Elec1.5mmUL 74695.0 °C
RTI Imp1.5mmUL 74695.0 °C
Physical propertiesTest ConditionTest MethodTest Result
Shrinkage rateASTM D9550.50-0.70 %
Water absorption rateASTM D570/ISO 620.22 %
Melt Volume Flow Rate (MVR)280°C/2.16kgISO 113317.5 cm3/10min
Shrinkage rateTD:4.00mmInternal Method0.50-0.70 %
Shrinkage rateMD:4.00mmInternal Method0.50-0.70 %
Water absorption rate23°C,24hrISO 620.22 %
Electrical performanceTest ConditionTest MethodTest Result
Surface resistivityIEC 60093>1.0E+15 ohms
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.